Another step, and most important one, is heat threatment. Heating up the blade to 830°c and cooling it down in oil hardens the blade and gives it its desired abilities like edge retention. After secondary heat threatment (tempering) at 280°c blade looses some of its hardness in exchange for flexibility. If all goes well, blade is on its way to be finished. #sword #hardening #blacksmith #viking #vikingsword